W751

Melting Route

Airmelted + Remelted

Product Description

BÖHLER W751 ISOBLOC is not a classic hot work tool steel, but a hardenable steel with an austenitic structure. Compared to quenched and tempered steels, the material does not generate its strength through a hardening structure with high carbon content and secondary hardening carbides, but through the precipitation of intermetallic phases from a tough austenitic matrix. BÖHLER W751 ISOBLOC is a chemically modified version of material number 1.2779 (X6NiCrTi26-15) and has proved to be ideally suited for many tool steel applications in cold and hot work (e.g., for extrusion liners) up to 750 °C and is therefore an economic alternative to superior nickel base alloys.

Property Features

Highly creep and corrosion resisting, precipitation hardening austenitic steel. Modified A286 for extrusion tools.

Technical Specifications

Material Numbers


~1.2779 ~X6NiCrTi26-15


Chemical Composition

Chemical composition (average %)
0.02 ≤ 0.20 1.40 15.00 1.25 25.00 0.30 2.80 0.25

Applications

Available product shapes

  • Open Die Forgings